TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Thu, 17 Jun 2010 08:08:54 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeff Popp <[log in to unmask]>
Subject:
From:
Jeff Popp <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (178 lines)
The IPC 610 does not require any wetting of solder on the solder destination side pad. All that is needed is 75% vertical fill of the PTH with 270 degree wetting lead to barrel for class 2 and 330 degrees for class 3.

Best Regards,
Jeff
 
Jeff Popp
Quality Assurance Technician
Compunetix
2420 Mosside Blvd.
Monroeville, PA 15146
(412) 858-6184

 
 

"Every right implies a responsibility; Every opportunity, an obligation, Every possession, a duty." ~ John D. Rockefeller

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, June 17, 2010 8:02 AM
To: [log in to unmask]
Subject: Re: [TN] Query on shelf life of PCBs & impact on solderability

Uppina,
Wow! LOTS of questions. I can only answer some.

1) Yes, generally ENIG boards store better than HASL boards.  HASL board solderability decreases because of growth of oxide and growth of intermetallic.  If the HASL layer is thin the intermetallic can reach the surface sooner and then, well, it ain't going to solder.

Vacuum packing can increase the shelf life of finishes that can oxidize.  This assumes excellent packaging, not stored so long there are intermetallic problems, etc., etc.

For a  lot more on this get the IPC series of docs on surface finishes. I can't remember the numbers, but I am sure someone else will respond with those.

2) Photos to TechNet get stripped out.  Either sent to Steve Gregory or post on the IPC site.
Question to you: what IPC class of product are you building?

Bev
RIM


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Uppina Nagaraj
Sent: Thursday, June 17, 2010 7:30 AM
To: [log in to unmask]
Subject: [TN] Query on shelf life of PCBs & impact on solderability

Dear All,

I have 3 queries in all.....

1. One of our customer has changed the surface finish from HASL
   to ENIG. Their main reason for this change was that they
   have had a bad experience with storage of HASL finished boards
   (the reason for which is not shared with us). They had encountered
solderability problems on the HASL finished board which they
   had stored for a period of time.

   Their expectation with Gold plated surface is the storage
   of the PCBs can be for a longer period of time as compared to
   HASL finish.

   Initially they had a requirement for 1micron thick electrolytic gold, 
but later on they changed the requirement for an ENIG process with 
gold around 0.05 to 0.10 microns.

   Now my question......

   Is there any guideline on the shelf life of the PCBs (with regard to
solderability) of the following surface finishes....

   a) ENIG
   b) HASL
   c) Immersion Tin
   d) Electrolytic Ni and electrolytic gold with Gold thickness
      of 1.0microns

   Will vacuum packing help to extend the shelf life?

2. One of our customer is doing hand soldering of PCBs with ENIG finish.
   They're inserting a strand of tinned Copper wires from component side
and later on using soldering iron to do the soldering from the solder
side.

   The solder is able to flow up from solder side to component side, but
the solder is unable to complete wet the pad on the component side.

   I've attached the photos of example of the phenomenon. These photos are
without the wire, I've just used bare PCBs to do the soldering to
illustrate the phenomenon.


   Now my question....

   a) Will increasing the volume of the solder help in complete wetting
      of the pads on the component side?
   b) Any other way to get a full coverage on the pads on the component
      side.

3. This question is about the same customer which I've mentioned in
   para 2 above, is doing hand soldering. In one of the stage of
   component assembly, they're (hand) soldering a flexible PCB
   on the ENIG finished rigid PCBs.

   They have a unique practice during this stage of soldering. They've
explained to us that this particular component is very sensitive to
high temperature and hence the soldering iron temperature is set at
210Deg C. They're using Sn60/Pb40 solder for this soldering operation.
After the soldering iron achieves 210Deg C, they're  turning off the
power to the soldering iron and doing the soldering of the flexi PCB
onto the rigi PCBs. We'll not know the actual
   soldering iron temperature at the point of contact.

   They've complained to us that the soldering is poor.

   We know that the melting temperature of solder is around 183deg C. But,

   is there any guideline on the minimum temperature for soldering to get
a good flow of solder and completely wetted solder?

Thanks for your inputs in advance.

Best Regards,
U.Nagaraj
MICROPACK Ltd,
Bangalore, INDIA.






______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2