TECHNET Archives

January 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
James Mahoney <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, James Mahoney <[log in to unmask]>
Date:
Tue, 4 Jan 2011 09:13:23 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (132 lines)
We always allow the PCB fabrication house to determine the pallet size for best manufacturing panel utilization based on their panel sizes and your proposed quantities.

Have them send it back for approval prior to releasing the job to the floor.

Thank you, Jim Mahoney 
Quick Turn Flex Circuits, LLC 
Applications Project Manager 
P# 603-821-7071
M# 603-305-6250 
www.quickturnflex.com
 Please consider the environment before printing this e-mail
** This email and all attachments have been scanned prior to being sent** 
Confidentiality Notice: This page and any accompanying documents contain information that is confidential, privileged or exempt from disclosure and is intended for the exclusive use of the addressee. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution or use of the contents of this information in any manner is strictly prohibited.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carl VanWormer
Sent: Monday, January 03, 2011 7:16 PM
To: [log in to unmask]
Subject: [TN] Looking for guidance on specifying panel of small PC boards

I have created a file ( http://www.cipher.com/Panelization02.jpg) that
is my guess at a PCB panel that will meet the following goals.

1.       A bunch of boards to reduce handling costs.

2.       Not too much waste.

3.       Side rails to keep the system from being too "wobbly" (that's a
technical term).

4.       Routed slots between boards to minimize twisting forces during
hand de-paneling.

 

The circuit boards will be made from .062" FR-4, and are each
2.875"x1.125".  the surface mounted parts will be placed, then fed to
the IR re-flow oven for the first pass of processing.  Then, the
through-hole connectors will be added at both ends of each board and the
panel will be wave soldered to attach the connectors.  The board will go
through the wave in the direction of the long axis.

 

My picture has interior single lines representing V-Scores, and thick
gray lines representing routed slots between pairs of boards. My goal is
for hand separation of the boards, with minimal forces on the chips on
the interior of the board area.   My hope is that one of the long side
rails (green) can be broken off, then each pair of boards can be snapped
from the other long side rail (green), then the pairs of boards can be
snapped apart.

 

I am making a lot of guesses from things I've seen before.  I'm looking
for guidance on how to specify panels that will be considered "good" by
all parties involved in the processing chain.  Are there published
documents that can help me look like an expert (without too much work on
my part)?

 

Thanks,

Carl

 

 

 

 

Carl Van Wormer, P.E., AE7GD

Senior Hardware Engineer

Cipher Systems

1800 NW 169th Place, Suite B-100

Beaverton, OR  97006

Cipher Systems (503) 617-7447 x 5163

Direct Line (503) 425-5163

[log in to unmask] <mailto:[log in to unmask]> 

This message may contain confidential and/or proprietary information,
and is intended for the person/entity to whom it was originally
addressed. Any use by others is strictly prohibited.  If I sent this to
you by mistake, please be nice and delete it, then tell me of my mistake
so I can send it to the right person.

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2