TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
"<Rudy Sedlak>" <[log in to unmask]>
Date:
Fri, 7 Dec 2001 11:07:46 EST
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (39 lines)
Greg:

You have discovered one of the great secrets of the industry....

The ammoniacal etch replenishers arrive with widely varying contents.

I consulted for a distributor of this chemistry, and had the same sort of
problems, and started analyzing the incoming stuff, and was stunned.  The
vendors can get away with it because virtually nobody analyzes their incoming
replenisher.

The vendors specs are usually wider than they ought to be, and they
frequently do not even meet their own specs.  (As a chemical vendor, I can
tell you that the most casual QC can keep any ingredient within 1% of
target....wider than that is self-serving)

Now, this caveat, the experience I write about above is 10+ years old, so, it
MAY no longer be applicable...however, if I were to bet, I would bet it has
not changed.

And incidentally, the chloride level does not change in the etching process,
so, there is no "controlling" it, assuming that you are not adding anything
to the replenisher.

Good luck.

Rudy Sedlak
RD Chemical Company

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2