TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Kerry McMullen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 16 Aug 2007 12:15:28 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (92 lines)
Hi Amol,
I have only been able to do it one pin at a time after total destruction 
of the connector body (If there is a connector body). 
I would double check the specto hole size.   Also, see if your PCB housr 
used the recommended pre-drill for the pree-fit plated hole.  This is 
critical. 
Some of the larger connectors I have worked with are up to 500 press-fit 
pins.



Kerry McMullen
Principal New Product Mfg. Engineer
LTX Corporation
825 University Avenue
Norwood, MA 02062-2643
(T) 781-467-5468
(C) 508-631-1832
(F) 781-461-0993



"Kane, Amol (349)" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
08/16/2007 11:45 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Kane, Amol (349)" <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Press Fit Connector rework






Dear Technetters,
Is anybody aware of ways to remove press fit connectors once they are 
inserted in the PTHs??. We have a situation where the connector is 
removing plating from the PTHs as well as removing the annular ring on the 
outside of the holes. The surface finish is ENIG. So far the investigation 
has revealed that the hole size and the pin size is within tolerance. 
While we are determining the root cause, we also need to see if there is a 
way to rework these boards.

I have some pictures which I can post if anyone wants to take a look.

Thanks in advance,
Amol



CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2