TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 29 Jun 2006 10:02:36 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (59 lines)
Poh,

I can see 2 reasons:
you are not heating enough. Are you measuring the temperature under the BGA? You need to peak at about 240C. Of course, if your PCB is not capable, it might get damaged.
you are not using the right tacky flux. You need lead-free capable flux, the SnPb one will decompose at these high temps.

Regards,

Ioan

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Poh Kong Hui
Sent: Thursday, June 29, 2006 9:55 AM
To: [log in to unmask]
Subject: Re: [TN] LEADFREE BGA - electrical continuity issue


Hi Technetter,

I recently faced issues with BGA of leadfree.
In the past, when we rework BGA (tine-lead), we sometime make short cut by
simply applying some paste flux, mount the BGA and reflow, it works
perfectly well on the electrical continuity.

Somehow, it seems using the same method does not work well on leadfree BGA.
Sometime, there is no issue with the electrical continuity, and sometime
there is problem with it.

We also do sometime apply (tin-lead) paste on the BGA pads, but it has the
same symptom.

We do X-ray, but not able to determine much from the X-ray picture.

Can someone advise me what had happened & how to solve such problem.

Thanks in advance.

KH Poh

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2