TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Tue, 6 Apr 2004 10:41:29 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Phil Nutting <[log in to unmask]>
Parts/Attachments:
text/plain (57 lines)
Brian,

How about using some of the "No-Alox" electrical "grease" that is used when connecting aluminum wires to copper wires on our house wiring?  The electric company uses this stuff all the time on the aluminum wires that come from the utility pole in the street that are connected to the copper wires that go to the power distribution panel in the house for the sole purpose of preventing dissimilar metal corrosion.

Let me know if you need more manufacturer's info.  Your local electrical supply house should have this in stock.

Phil Nutting

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brian Ellis
Sent: Tuesday, April 06, 2004 10:31 AM
To: [log in to unmask]
Subject: [TN] Slightly OT for conformal coating experts.


I'm on the point of ordering a solar panel installation. The PV panels
are set into an aluminium profile framework, held together with
stainless steel (presumably 18/8 alloy) screws etc. The installation has
a projected lifetime of ~40 years. In this timeframe, I'm a wee bittie
worried about dissimilar metals, exposed to the weather, causing
corrosion. Granted the surface area of the Al is ginormous, compared to
that of the hardware, so that the corrosion will not be localised.

The weather here is typically 9 months hot and dry (say, 25 - 47°C, 45 -
20% RH resp.), aggravated by direct exposure to the sunlight. The other
three months are cool with intermittent heavy rain (say, 0 - 25°C, 45%++
RH).

Would it help to paint onto the hardware (not the profiles) an epoxy
coating, after the screws have been tightened, to reduce the risk of
long-term corrosion? If so, what type? How does the epoxy stand up to UV
exposure over the years?

TIA

Brian

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2