Hi
IPC-4552 calls for XRF to measure ENIG plating thickness. But, this method can only be applied to surface pads. How can we assess the quality of the plating in via barrel ? (poor plating would compromise mechanical strength and resistance to corrosion)
Thanks for your insight
Fabien