Hi Steve,
IMHO .002 webs are pretty tiny, I think .003 is pushing it too. I would
expect problems with anything below .004.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly
Sent: Thursday, July 10, 2014 8:14 AM
To: [log in to unmask]
Subject: Re: [TN] Solder mask tape test
Hi All,
Need some opinions please. The S/M web is .002 to .004 wide. Thanks.
Steve Kelly
From: Steven Kelly
Sent: July-09-14 1:56 PM
To: 'TechNet E-Mail Forum'
Subject: Solder mask tape test
Hi All,
Should I have issues passing the IPC-TM-650 Method 2.4.28.1 when the
S/M web is .002 to .004?
Regards Steve Kelly
Phone(O) (416) 750-8433
Phone (C) (416) 577-8433
If the recipient to whom this e-mail is sent has an NDA with PFC
Flexible Circuits Limited this e-mail is considered confidential and is
subject to any NDA agreements between the respective parties.
See PFC on "How its' Made" in Canada on July 7th at 8 p.m. on the
Discovery Channel
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|