Thanks Doug,
He is in an auto manufacturing OEM company now and he is trying to learn a new product type. In telecom we don’t use conductive epoxy so I have never attempted to look into it. The photo he sent me looks sloppy to me. They are using needle transfer and they may have a viscosity issue so they are getting what appears to be stringing. I appreciate your comments. Thank you,
RUSSELL NOWLAND
Nokia - (US)
REPAIR STRATEGY & SUPPLIER MANAGEMENT
Virtual Office Oklahoma
T: +1 972 477 8665
M: +1 405 203 0034
[log in to unmask]<mailto:[log in to unmask]>
From: David Hillman [mailto:[log in to unmask]]
Sent: Monday, June 13, 2016 1:44 PM
To: TechNet E-Mail Forum; Nowland, Russell (Nokia - US)
Subject: Re: [TN] Conductive Epoxy Endpoint Requirements
Hi Russell - I don't know of an industry specification (like IPC JSTD 001) that covers a conductive epoxy joint. We always put the required criteria on our drawings and do not reference any specification.
Dave Hillman
Rockwell Collins
[log in to unmask]<mailto:[log in to unmask]>
On Mon, Jun 13, 2016 at 1:30 PM, Russell Nowland <[log in to unmask]<mailto:[log in to unmask]>> wrote:
Hey all,
I was asked a question which is not something I have not dealt with. But being a nice guy I told them I would post a message on the TechNet and see if any of you have dealt with this. My friend is building flex circuits using conductive epoxy instead of solder. He was asking me what the endpoint requirements were for conductive epoxy because he could not find anything in IPC-610F. I did find IPC-3406 but that does not have conductive epoxy endpoint type requirements. I am not sure what to call the joints other than fillets but he is looking for that type of info. If you know what or where the industry standard for conductive epoxy available I would appreciate you letting me know so I can pass it on. Thank you,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|