TECHNET Archives

April 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Tue, 3 Apr 2018 13:43:34 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (139 lines)
Hi Guy,

Yes, I'm afraid you may be right. When you have a government who fully
supports it's manufacturing capabilities as strategic, and focuses great
effort in advancing and improving it's knowledge and technology, we'll
always be left behind unless we put forth the same effort. Things may be
changing though, we'll see...

Steve

On Tue, Apr 3, 2018 at 12:18 PM, Guy Ramsey <[log in to unmask]> wrote:

> nice looking stuff. I fear we are getting left behind.
>
> On Sun, Apr 1, 2018 at 11:59 PM, John Burke <[log in to unmask]> wrote:
>
> >
> >
> >
> >
> >                 Contact details::
> > TEL:86-519-86225678  FAX:86-519-86558599E-mail:
> [log in to unmask]
> > cnhttp://www.quickchina.com.cn
> >
> >
> >
> >                 Sent from my iPad Pro
> >
> >
> >
> >
> >
> >
> > On Sun, Apr 1, 2018 at 7:11 PM -0700, "John Burke" <[log in to unmask]>
> > wrote:
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >                 Used to be made in US but now they come from China I will
> > send you contact details when I get to the office tomorrow.
> >
> >
> >                 Sent from my iPad Pro
> >
> >
> >
> >
> >
> >
> >
> > On Sun, Apr 1, 2018 at 5:10 PM -0700, "Guy Ramsey"  wrote:
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
> > I  am not aware of any brands. Who makes them?
> >
> > On Sat, Mar 31, 2018 at 11:39 AM, John Burke  wrote:
> >
> > >
> > >
> > >
> > >
> > >
> > >                 Actually using a laser rework station for this.
> > > It keeps all surrounding components below melting point even on a
> double
> > > sided mirror imaged BGA design.
> > > Best regards,
> > > John
> > >
> > >
> > >                 Sent from my iPad Pro
> > >
> > >
> > >
> > >
> > >
> > >
> > > On Fri, Mar 30, 2018 at 1:19 PM -0700, "Guy Ramsey"
> > > wrote:
> > >
> > >
> > >
> > >
> > >
> > >
> > >
> > >
> > >
> > >
> > > We are seeing more and more designs where it is not possible, with our
> > BGA
> > > reworkstation, to remove or reinstall components and not reflow
> adjacent
> > > parts, or in some cases, part on the opposite side of the assembly.
> > > What action do you all take to mitigate the resulting conditions?
> > >
> >
>



-- 
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133

-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 

ATOM RSS1 RSS2