TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Blair Hogg <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Blair Hogg <[log in to unmask]>
Date:
Wed, 12 Nov 2008 09:09:56 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (31 lines)
When I was a kid I had this electroplating system that was a close 
approximation to the plating pens. Several bottles of different plating 
solutions, a plastic housing with batteries that had a foam applicator 
and a clip lead. You would clip the lead to the part you wanted to plate 
and paint the plating on. And it worked pretty well!

Blair

On Wed, 12 Nov 2008 07:06:00 -0600, Stadem, Richard D. 
<[log in to unmask]> wrote:

>I would let him do it.
>I do chemical plating and plating rework on occasion, as needed. I also
>know of a few companies that do this as a standard benchtop 
production
>process. You can buy plating kits and do it yourself, if you so desire.
>I have plated gold, nickel, silver and copper buildup. If done properly,
>it is just as "good" or reliable as the original bath. Check out
>http://www.hunterproducts.com/
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2