Conformal coating will provide protection from the outside conditions. This
coating is put on the board after the assembly process.

Kenneth McKee
PCB Designer
MJS Designs, Inc.
4130 E. Wood Street
Suite 100
Phoenix, Arizona 85040
(602) 437-5068
(602) 437-5299 FAX
mailto:[log in to unmask]

 -----Original Message-----
From:   Dean Hunt [mailto:[log in to unmask]]
Sent:   Monday, November 20, 2000 1:16 PM
To:     [log in to unmask]
Subject:        [TN] PCB Corrosion

Is anyone having problems with PCB corrosion. We have a number of products
which are showing signs of corrosion on the copper tracks and planes. The
products concerned are in non-air conditioned  environment and varying
humidity situations. Does anyone know of a suitable method to protect PCBs
from external elements. I am keen to hear of any known solutions to this
problem.

Thanks


                                 Dean Hunt
                           CAD Solutions Manager
----------------------------------------------------------------------------
---

    Invensys Energy Systems (NZ) Limited, 39 Princess St, PO Box 11-188
                      Christchurch 8030, New Zealand
             Phone: (++64) 3 343-3314, Fax: (++64) 3 348-5100
                       Phone: (++64) 3 343-7471,DDI
                   Email: [log in to unmask]
                 Website: http://www.invensys-energy.co.nz
----------------------------------------------------------------------------
----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2