TECHNET Archives

September 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 26 Sep 2013 10:29:56 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Rueda, Ernesto" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
From:
"Rueda, Ernesto" <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)

Hi all,

I am seeking recommendations from the experts of this forum about tarnishing of the PCB board finish with Immersion Silver.

Please enlighten me about the minimum thickness of silver metal on top of the copper layer. 
What is the maximum process time limitation to build these boards?

Our SMT machine was down for more than 3 days that went through the weekends and the boards were not completed. 
It is possible that varying temperature and humidity affected some of the assemblies. 
We have problems with testability at some test points because of the tarnishing issues.

We are planning to send out some panels for plating thickness test and contamination tests as well.
Any provider that you may recommend?


Thank you in advance.

Ernesto


Ernesto V. Rueda   |   PELCO by Schneider Electric   |   SMT Process Engineer
Phone: +1 559-292-1981 ext. 3848  |   Fax: +1 559-388-3781  |   Mobile: +1 559-333-3913
Email: [log in to unmask]    |   Site: www.pelco.com   |   Address: 3500 Pelco Way, Clovis, CA  93612-5699 USA
 please consider the environment before printing this email

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2