Dave Rooke,

I don't know how accurate the measurements were on the immersion
gold, but they were made with a Fisher x-ray fluorescence meter. Their
phone number is 800-243-8417.

Vic Beldavs
414-362-2797
[log in to unmask]

***************************************************************************