TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 13 Jan 2009 17:15:59 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Larry Dzaugis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=ISO-8859-1
From:
Larry Dzaugis <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
What is a simple test to tell the difference between alcohol and water based
fluxes?
Both are 3% solids flux.

I am running both fluxes in the same machine.
The concern is that the wrong flux is loaded during a change over.
They behave so differently that the use of the wrong one will result in
badly soldered boards.

Our long term solution is seperate flux tanks and spray nozzels if it
continues with bar code verified replenishment.

In the mean time what would be a quick test?

The weight of an alchol flux on the PCB is inconsistent due to evaporation.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2