TECHNET Archives

October 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 1 Oct 1998 11:42:27 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (39 lines)
In a message dated 10/1/98 8:11:35 AM Pacific Daylight Time,
[log in to unmask] writes:

<< Steve,
        What would you use x-ray for on initial set-up of a process?

        If process is verified during the initial set-up (for arguments sake
 we can say by x-ray) --What were you intending to tell you that it was under
 control while running, How would you monitor it?
 Semper Fi
 Tom >>

Hi Tom,

     What I would use it for on initial set-up, is to verify placement after
reflow, and that there were no really unusual voids, bridges, or things of
that sort beneath the package. I know the jury is still out on what it is you
see with xray being a defect or not.

     As far as what I would monitor during the rest of the process, one would
assume that if I were making sure that I was putting the proper amount of
paste down accurately, placing the components in the same place I did on my
first board, and using the same reflow profile that I used on my first board,
I should obtain the same results...no?

-Steve Gregory-

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2