Jim,
Automata in Sterling, Va. (a former employer of mine) does microvia,
blind and buried technology. I know that they have in-house capability
for laser drilling and immersion gold plating. You can reach Keith
Frymyer in Sales @ 703-450-2600 for details.
Anne Ledger
EMDS, Inc.
> On Mon, 23 Aug 1999 15:49:41 -0600 Jim Kittel
> <[log in to unmask]> writes:
> >Fellow TechNetters,
> >
> >We are are moving into the assembly/design of circuit card assemblies
> >using
> >micro via technology and I need a lead on some PWB vendors that can
> >fabricate boards with buried or blind micro vias. These designs will
> >require vias in the 0.004 to 0.008 inch diameter range with 0.004
> inch
> >trace
> >widths. I would like to find a supplier that can do the entire
> >process in
> >house. The finish will be nickle/immersion gold, typically FR-4 or
> >polyimide and we are talking small order sizes.
> >
> >Any ideas on who to contact?
> >
> >Jim Kittel
> >
> >##############################################################
> >TechNet Mail List provided as a free service by IPC using LISTSERV
> >1.8c
> >##############################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> >following text in
> >the body:
> >To subscribe: SUBSCRIBE TECHNET <your full name>
> >To unsubscribe: SIGNOFF TECHNET
> >##############################################################
> >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> >additional
> >information.
> >If you need assistance - contact Gayatri Sardeshpande at
> >[log in to unmask] or
> >847-509-9700 ext.5365
> >##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at
> [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|