TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Date:
Thu, 6 Oct 2005 09:51:43 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Stadem, Richard" <[log in to unmask]>
Parts/Attachments:
text/plain (96 lines)
Franklin is correct.
Refer to IPC 7095 page 66 fig. 7.5 and Table 7.3. This shows how to
dimension the score such that the amount of remaining material desired
is known (dim. A). If you keep this remainder at less than .015" for
standard thicknesses of .062" it will be OK. But it cannot be too small,
or the remaining web will break easily during normal handling. For
thicker boards it should be no more than .015"-.018" remaining, as this
provides sufficient strength but will still singulate easily.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin D Asbell
Sent: Wednesday, October 05, 2005 6:11 PM
To: [log in to unmask]
Subject: Re: [TN] PCB Score Depth

You will find it referenced briefly in 6012, it might even be in IPC
2221 but dimensions would not be included.

Typically the user (buyer, customer, assembler, etc) would include their
requirements in the fab drawing or spec.

A v-score of 2/3 board thickness is most common; however, this is most
often used for .049 - .062 thick boards. 2/3 rule would not work well
with a .150 thick board and would cause all sorts of problems on an .030
board.

You can mix score and rout (web cut) and can also skip-score (or jump
score) which is most common on thinner boards.

Score depth like nearly everything board related has many variables
which would control it, for example, will an post-score machine be used,
will the array be in a frame during assembly, individual piece size and
number in the array, are components attached close to the edge, near the
score line, are there through hole components, are components attached
to one side or both.

Those and a myriad of other variables will dictate the type and depth of
score.

If you provide some specific features we would be glad to offer more
insight.

Franklin


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joel Mearig
Sent: Wednesday, October 05, 2005 4:52 PM
To: [log in to unmask]
Subject: [TN] PCB Score Depth

Is there a specification for score depth on PCBs? In other words does
one always leave the same amount of web after scoring regardless of the
board
thickness or is it a percentage of board thickness? Thanks
Joel


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest