TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Guenter Grossmann <[log in to unmask]>
Date:
Wed, 29 Nov 2000 04:10:24 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Fish <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
David Fish <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
Guenter:  Should the rate of temperature decrease be the same as the rate of temperature increase that you quote?  Dave Fish

Guenter Grossmann wrote:

> David
>
> This translates to nothing because:
> - We don't know the temperature swing in your application.
> - 5 min. dwell time at -55 degC is as much as nothing, thus no strain is induced.
> - 10 degC / min is very fast below 20 degC and you are very likely to activate degradation mechanisms that do not occur in reality.
>
> Running a test
> - 0 / 120 degC
> - 4 degC / min up to 20 degC
> - 10 degC / min above 20 degC
> - dwell time of 5 min at 120 degC
> - dwell time 30 min at 0 degC
>
> would give in my opinion the possibility for a rough estimate of the lifetime in a realtime environment by
>
> Nfr = Nft ( dTt  / dTr )exp1.7
>
> Nfr = Number of cycles to failure reality
> Nft = Number of cycles to failure test
> dTr = Temperature swing reality
> dTt = Temperature swing test
>
> Best regards
>
> Guenter
>
> Guenter Grossmann
> Swiss Federal Institute for Materials Testing and Research EMPA
> Centre for Reliability
> 8600 Duebendorf
> Switzerland
>
> Phone: xx41 1 823 4279
> Fax :      xx41 1823 4054
> mail:     [log in to unmask]
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2