Colin,
How much heat you moving? Does thermal resistance at the heatsink junction
have to stay low, or extremely low. If you have to move a lot of heat,
Chomerics has a process called Power Site that allows you to solder your
device directly to the heatsink (see
http://www.parker.com/chomerics/products/documents/powersite_cat.pdf.).
Have you investigated thermally conductive adhesive tape? They don't have
the mess of the thermal adhesives and they are repairable. Check out 3M
http://www.3m.com/us/mfg_industrial/adhesives/html/tc_selector.jhtml or
Bergquist http://www.bergquistcompany.com/therm.htm, they might give you
some thermal management ideas.
Good Luck,
Gary Camac
----- Original Message -----
From: "Colin Weber" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, August 12, 2002 9:06 PM
Subject: [TN] Thermal Potting Mix
> We have a scenario where we want to put string of rectifier diodes in
> series, onto
> an aluminium heatsink, to conduct heat from them. What we envisaged doing
is
> soldering these diodes onto a single sided circuit board and potting this
> assembly
> onto the heatsink.
>
> My question is what is the most suitable thermally conductive potting mix
to
> use for this case, and will not let loose, or break free from the
aluminium
> over
> time?
>
>
> Regards,
>
> Colin Weber
>
> Regards,
>
> Colin Weber
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|