TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Hfjord <[log in to unmask]>
Date:
Mon, 7 Aug 2006 23:49:18 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (59 lines)
Tom,
standards are nice to have, but one needs to have own opínions about what is
good and bad. What you describe calls for extra attention, would suggest a
wetting balance test and also an investigation of the soldered caps by means
of cross section and SEM/EDS. The 'demarkation' line can be coarse Lead
crystals or crystals of intermetallic nature, often with a greyish touch,
and with little negative impact. But to be sure that it ain't debris from a
bad wetting or dewetting, I'd look a little extra as like I said earlier.
Ingemar Hernefjord
Ericsson Microwave Systems


----- Original Message -----
From: "Gervascio, Thomas" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, August 07, 2006 9:39 PM
Subject: [TN] Chip component solderability requirements


I have a question about the solderabilty requirements on chip resistor
and capacitors per J-STD-001D. I have solder wetting up to the top of
chip components where in come cases there is a distinct line of
demarkation. In other cases the solder wets over the end termination of
the part and has a smooth wetting angle. Is a visible line of
demarkation rejectable per J-STD-001 soldering requirements (para 4.14).
The requirment is for a 50 percent solder fillet height and although a
smooth wetting angle is perferred - is a line of demarkation (non
wetting vs dewetting) a cause for rejection? I am using 63/37 eutectic
solder so the alloy is not exotic.

Thanks much
Tom Gervascio
Senior Process Engineer
Sypris Electronics

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2