The main issues are, deterioration of the flux characters and oxidation of
the solder particles.
Reuven
On Mon, Jan 16, 2012 at 10:40 PM, Karen Tellefsen <
[log in to unmask]> wrote:
> sorry wrong email
> Karen Tellefsen - Electrical Testing
> [log in to unmask]
> 908-791-3069
>
>
>
>
>
>
> Re: [TN] Expired Solder Paste
>
>
> Karen Tellefsen
> to:
> TechNet
> 01/16/2012 02:54 PM
>
>
>
>
> Sent by:
> TechNet <[log in to unmask]>
> Please respond to TechNet E-Mail Forum, Karen Tellefsen
>
>
>
>
>
>
>
>
>
> thanks
>
> Karen Tellefsen - Electrical Testing
> [log in to unmask]
> 908-791-3069
>
>
>
>
>
>
> Re: [TN] Expired Solder Paste
>
>
>
> Matthias Mansfeld
>
> to:
>
> TechNet
>
> 01/16/2012 01:37 PM
>
>
>
>
>
> Sent by:
>
> TechNet <[log in to unmask]>
>
> Please respond to TechNet E-Mail Forum, Matthias Mansfeld
>
>
>
>
>
>
>
>
>
> On 16 Jan 2012 at 8:17, Stadem, Richard D. wrote:
>
> > You can re-certify expired solder paste per J-STD-005 section 6.0.
> > Used the form attached therein, and follow the appropriate test
> > methods (also listed at the end of J-STD-005, #2.4.34, 2.4.34.1,
> > 2.4.34.2, 2.4.34.3 for the viscometer you wish to use. You should
> > always perform first article testing, monitor your PPMO, etc., and
> > document all product run with the re-certified paste.
>
> For what it's worth, a good solder paste, stored under good
> conditions may work well even years after expiration. Been there,
> done that without re-certification (don't worry, no customer
> projects, just some own DIY-stuff....). For this stuff I use still
> the same 1kg-jar with old Sn63Pb Alpha RMA390D3K from 2003.... prints
> well, tacky like new, and visually perfect, shiny solder joints...
> even 8 years after expiration date.
>
> Best regards
> Matthias Mansfeld
> --
> Matthias Mansfeld Elektronik * Leiterplattenlayout
> Neithardtstr. 3, 85540 Haar; Tel.: 089/4620 093-7, Fax: -8
> Internet: http://www.mansfeld-elektronik.de
> GPG http://www.mansfeld-elektronik.de/gnupgkey/mansfeld.asc
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] 847-615-7100
> ext.2815
> -----------------------------------------------------
>
--
Best Regards,
*Reuven Rokah*
Mobile: 972-52-60-120-18
Tele-fax: 97239360688
<http://www.rokah-technologies.com/>[log in to unmask]
[log in to unmask]
www.rokah-technologies.com
**
This e-mail message is intended for the recipient only and contains
information which is CONFIDENTIAL and which may be proprietary of Rokah
Technologies. If you have received this transmission in error, please
inform me by e-mail, phone or fax, and then please delete all of the
original files and all other copies exist.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|