Hi,
In the early days of SMT, many people tried lower melting point temp solders
on the second side. It is common practice now to use the Sn/Pb eutectic on
both sides relying on surface tension to hold the components. I personally
do not know of anyone using 2 different melting point solders on
double-sided boards these days. In order to attain lower melting points,
one must use a bismuth-containing alloy. Customers were not happy with the
less than shiny joints.
Chris Christian
Indium Corporation of America
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jerry Mosur
Sent: Wednesday, February 13, 2002 10:09 AM
To: [log in to unmask]
Subject: [TN] Reflow Process
Hello,
As a part of our preparations to set up an internal SMD line, I would like
to get your opinion on the following topic.
What are the problems, if any, associated with reflowing the double sided
SMT board using solder paste with different melting points for top and
bottom.
Is this a fairly common process?
If not what would you recommend as a best assembly process for double sided
SMT boards?
Thanks in advance,
Jerry
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|