Hi Steve -
From your description it sounds suspiciously like one of the pieces of
laminate in that particular board may have missed a cleaning, rinse or prep
step at the board fabricators place. Were these boards panelized at the
lamination stage - if so, there may be some others which are at risk. The
board fab house is probably your best asset toward determining cause on this
one.
Kelly
-----Original Message-----
From: Stephen R. Gregory <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Wednesday, February 09, 2000 11:15 AM
Subject: [TN] Delamination
>Hi ya'll!
>
>We just finished building a lot of 48-boards through SMT. Out of that 48
>there was one board that we just discovered a big delamination blister on
the
>backside...it's about 1.5" wide and maybe 2.5 - 3" long. There was no
rework
>done on the board, and it was reflowed under the same profile in a
>Conceptronic HVA-70 that the rest of them were...and they don't exhibit any
>problems. There no sign of overheating at all around the blister, and the
>silkscreen is nice and bright white...we just have this big blister. What
>might cause that? The boards are polyimide. We didn't bake them, and they
>were real fresh boards date code was 0300. Like I said, it was the only
board
>that had a problem...the rest are fine.
>
>TIA
>
>-Steve Gregory-
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|