JF,
Here's an input from my colleague, Blaine Partee...
The list of materials at the beginning of IPC-TM-650 is quite accurate.
With the exception of vacuum impregnation equipment and metal bonded diamond
discs both high and low volume microsectioning requires equipment
specifically for the preparation of metallographic samples.Many companies
make tabletop grinding/polishing wheels. Consumables such as epoxy, paste,
molds, and polishing powder can be purchased in low quantity. It may be wise
take a short course on sample preparation. It will save you from much
headache caused by poor sample preparation and interpretation.
If you have any additional questions, give us a call.
Good Luck
Lee Whiteman
Senior Manufacturing Engineer
ACI / EMPF
Telephone: (610) 362-1200; Ext. 208
FAX: (610) 362-1290
E-Mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bissonnette,
Jean-Francois
Sent: Friday, January 19, 2001 3:13 PM
To: [log in to unmask]
Subject: [TN] Microsectionning
Hello Technetters,
IPC-TM-650 describes how to do microsectionning of PCB. Is this a
procedure
that can be done In-hous with any regular tooling.
We don't need microsectionning very often and it would be interesting if
we can do
it on site without too much trouble...
Thanks for any input!
JF
WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged
and confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.
|
|
|