Hans
Provided it's lead-free :-)
Actually, I've found that cored solder hardly deteriorates. After all, oxygen is the
great deteriorator and oxygen cannot get to that flux core very easily. The metal may
be slightly oxidised but a wipe through a coarse cloth as you pull it off the reel is
sufficient to handle most of that. Perhaps low solids (<2% flux) wire may be less easy
to use as there may not be enough activator to handle excess oxides.
Brian
"Stephen R. Gregory" wrote:
> In a message dated 09/08/2000 11:41:52 AM Central Daylight Time,
> [log in to unmask] writes:
>
> > Hi ya Stevo!
> >
> > How about some rosin cored solder wire that has to be at least five years
> > old?
> >
> > Hans
>
> Hey Hans!
>
> Might be good for some fishing weights...hahahaha
>
> -Steve-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|