Good day, Luan
Here are some things to try.
If you can, try pre-heating the assembly using either a small oven or a
hot plate just prior to soldering. Make sure the operator wears some
type of gloves to protect their hands when handling to hot assemblies.
Try pre-heating to about 90 deg. C to 110 deg. C. Pre-tin the component
leads if necessary to aid in the wetting.
I suspect you are not getting topside fillets only because of the mass
of the assembly, so making sure the assembly is pre-heated while
soldering should fix the issue.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Luan Nguyen
Sent: Tuesday, August 26, 2008 9:27 PM
To: [log in to unmask]
Subject: [TN] solder vertical fill on thermal pad
Dear All,
we are having a problem about hand soldering (lead-free) for some PTH
parts mounted on thermal pad. Solder vertical fill is difficult to up
75%. Can you help us some conditions and technics related for this
problem.
Thanks
***************************
Nguyen Hoang Luan
QC&Training Supervisor
Spartronics VietNam Co, Ltd.
No.3, Street No.6, VSIP
Th An Dist., BDuong Prov., VN
Tel: (84-650) 784 890
Fax: (84-650) 784 891
Mobile: 090.3.667448
Email: [log in to unmask]
***************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|