Brent,
Don't know of any environmental issues but I would suggest you check for
adhesion.
My information is that Paralene seemingly will not work with no-clean
processed assemblies, flux residues and all that. I am sure that someone at
SCS will correct me if I am wrong.
Paralene is a great process but it is expensive and time consuming being
batch processing using a vacuum chamber. Unless otherwise specified, you may
well find that a conventional coating will do that job equally well but more
easily and at less cost.
Regards, Graham Naisbitt
__________________________________________________________________________
[log in to unmask]
Concoat Ltd
Alasan House, Albany Park
Camberley GU15 2PL UK http://www.concoat.co.uk
-----Original Message-----
From: Brent Alcorn <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 05 June 1998 13:12
Subject: [TN] Parylene Conformal Coating line requirements.
>Hi Everyone,
>
>The company I work for is looking at installing a Parylene conformal
>coating system. In an effort to obtain an unbias opinion I would like
>to know:
>
>1) What are the environmental issues ?
>
>2) How clean does the PWB substrate have to be (FR4)? Do we need a
>"CLEAN ROOM" and are there special pre-coating requirements?
>
>Thanks
>Brent Alcorn
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|