TECHNET Archives

January 2020

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 7 Jan 2020 10:47:37 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Grossmann, Günter <[log in to unmask]>
Message-ID:
Subject:
From:
Grossmann, Günter <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (45 lines)
We always buy Epoxy resin in a larger quantity and store it up to one year without any problems.

Best regards

Günter 



-----Ursprüngliche Nachricht-----
Von: TechNet <[log in to unmask]> Im Auftrag von Stadem, Richard D
Gesendet: Montag, 6. Januar 2020 20:33
An: [log in to unmask]
Betreff: Re: [TN] storage life of PCB microsection mold

Absolutely!


-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Bhanu Sood
Sent: Monday, January 6, 2020 11:10 AM
To: [log in to unmask]
Subject: Re: [TN] storage life of PCB microsection mold

And the microsectioned/prepped surfaces are protected from internal and external contamination.


> On Jan 6, 2020, at 11:44 AM, Stadem, Richard D <[log in to unmask]> wrote:
> 
> I would assume it is just about forever as long as it was potted within the shelf-live and pot life of the mold potting material.
> 
> 
> -----Original Message-----
> From: TechNet <[log in to unmask]> On Behalf Of R Saravanan
> Sent: Monday, January 6, 2020 10:16 AM
> To: [log in to unmask]
> Subject: [TN] storage life of PCB microsection mold
> 
> Dear all,
> 
> What is the storage life of the pcb microsection mold . How long we can preserve.
> 
> I am using long curing resin.
> 
> R.Saravanan