There are some numbers being thrown around for immersion Tin Thickness that
are a little unrealistic.

Getting 40+ microinches (1+ micron) is pretty difficult, to impossible on a
production basis.  It can be done in a lab, with a freshly made up bath, but
I have never seen even 50 microinches ever, and this is with any immersion
Tin process.

Is anyone even maintaining 40 microinches in production?

I suspect that you have to run your process pretty carefully to maintain 30+
as the bath gets old.

Will production people comment please?

Rudy Sedlak
RD Chemical Company

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2