TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge Hernefjord <[log in to unmask]>
Date:
Tue, 3 Apr 2012 16:35:33 -0400
Reply-To:
Message-ID:
Content-Transfer-Encoding:
7bit
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (171 lines)
Also:

  I thought this thread start because it was only certain caps on a board
that were discolored? I think it was related to caps towards the board
center.

 Maybe I am just confusing topics?

Bob K

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Tuesday, April 03, 2012 4:13 PM
To: [log in to unmask]
Subject: Re: [TN] Discolored Leads on D-Case Tantalum Caps

So, this manufacturer does not have control on his process and asks you to
accept discolored leads. Strange arguments. I have decades of experience
behind and I have seen that LEAD FINISH is one of the most frequent failure
sources.Just be careful.

Inge

On 2 April 2012 22:23, David Bealer <[log in to unmask]> wrote:

> Update:
>
> The manufacturer has replied that the discoloration is a normal result 
> of their aging process which uses heat and humidity (these are not 
> Tantalum caps but a Polymer Aluminum equivalent).  They stressed that 
> the discolored leads are still solderable, and as such were not defective.
>
>
> David Bealer  |  SMT Department Manager
> Phone: (217) 442-0611 ext. 6022  |  Fax: (217) 477-7134
>
> Watchfire Signs by Time-O-Matic Inc.
> [log in to unmask]
> www.watchfiresigns.com
>
> -----Original Message-----
> From: David Bealer
> Sent: Thursday, March 08, 2012 12:56 PM
> To: 'TechNet E-Mail Forum'; 'Steve Gregory'
> Subject: RE: [TN] Discolored Leads on D-Case Tantalum Caps
>
> I had the same thought - that the parts are "recycled".  These are not 
> Vishay.  The distributor certifies that these are genuine, and we have 
> now gotten the manufacturer involved.  They will have samples in their 
> hands tomorrow so hopefully we will have this all cleared up shortly.
>
>  -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: Thursday, March 08, 2012 12:23 PM
> To: [log in to unmask]
> Subject: Re: [TN] Discolored Leads on D-Case Tantalum Caps
>
> Hi David,
>
> Sorry about not getting this posted earlier, but I have not been 
> feeling well today, and just got around to checking my email. I have 
> your picture posted now though:
>
> http://stevezeva.homestead.com/discolored_leads.jpg
>
> I think what guy was referring to was a thread from a while back that 
> I started about a purplish tint that I saw with some SAC305 solder on 
> a gold plated board. Here was the picture:
>
> http://stevezeva.homestead.com/Trippy_Solder.jpg
>
> George Wenger was interested in analyzing it for me, and this was his
> report:
>
> http://stevezeva.homestead.com/FSC-5178.ppt
>
> But what I see with your caps is different I think. The purplish tint 
> that you are seeing maybe some of same sort of oxide that was in the 
> SAC305 solder that I saw, but I find it hard to believe that the 
> manufacturer would ship tantalum capacitors looking like that. I've 
> seen many, many reels of tantalum capacitors, and I can say that I've 
> never seen them come from the manufacturer looking like this. Do these
happen to be Vishay?
>
> One of the things that come to my mind is that these may be counterfeit.
> They almost look like they've been pulled off boards. You say that 
> they're straight out of the manufacturer packaging, but where did you 
> actually purchase them from?
>
> Just from the picture, I would be suspect of these parts...
>
> Steve
>
>
> -----Original Message-----
> From: Guy Ramsey
> Sent: Thursday, March 08, 2012 10:36 AM
> To: [log in to unmask]
> Subject: Re: [TN] Discolored Leads on D-Case Tantalum Caps
>
> Hi David,
> Steve is out today, not feeling well. He may monitor his mail.
> But, there was a thread a couple of weeks back about tin and purple 
> tint on the surface of solder.
> It might be of interest.
> Guy
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of David Bealer
> Sent: Thursday, March 08, 2012 9:32 AM
> To: [log in to unmask]
> Subject: [TN] Discolored Leads on D-Case Tantalum Caps
>
> I have some tantalum caps that the leads are so discolored (a brown to 
> purple tint to them) that the pick & place vision system is rejecting 
> all of them.  these are supposed to be 100% Sn plated, are MSL 3 
> rated, and these are new parts straight out of the manufacturer's 
> packaging with no signs of breach.  The leads also will wet out using 
> solder paste with OA flux.
>
> If I can get the machine to place these what reliability issues could 
> we be facing?
>
> I have a picture of several parts that I'll ask Steve to post.
>
> David Bealer  |  SMT Department Manager
> Phone: (217) 442-0611 ext. 6022  |  Fax: (217) 477-7134
>
> Watchfire Signs by Time-O-Matic Inc.
> [log in to unmask]<mailto:[log in to unmask]
> > www.watchfiresigns.com<http://www.watchfiresigns.com/>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask]
> ________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask]
> ________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask]
> ________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2