A 2 hour bake is not what IPC recommends for rigid flex. HDBK-001 says a
minimum of 6. Regards Steve Kelly
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Mahoney
Sent: June-23-08 1:06 PM
To: [log in to unmask]
Subject: Re: [TN] edge delamination flexible circuits assemblies
Without understanding the actual material being used it's difficult to tell.
I would recommend cleaning with alcohol and bake prior to any assembly @ 250
degrees for 2 hours and try and solder within 4 hours.
Thank you,
Jim Mahoney
Quick Turn Flex Circuits, LLC
Applications Project Manager
P# 603-821-6571
F# 603-821-5723
M# 603-305-6250
** This email and all attachments have been scanned prior to being sent**
Confidentiality Notice: This page and any accompanying documents contain
information that is confidential, privileged or exempt from disclosure and
is intended for the exclusive use of the addressee. If you are not the
intended recipient, you are hereby notified that any disclosure, copying,
distribution or use of the contents of this information in any manner is
strictly prohibited.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gabriela
Sent: Monday, June 23, 2008 1:11 PM
To: [log in to unmask]
Subject: [TN] edge delamination flexible circuits assemblies
What may cause the edge delamination of rigid/flex assemblies along the
edges of the flex connector?
We saw this defect only after cleaning the circuits in ABZOL .
Before assembly we are drying the circuits for several hours at 120C. Is it
possible that the cleaning process attacks the adhesive?
Are there recommendations for cleaning flexs?
Gaby
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|