Peter,
Provided your oven is a convective reflow system, you should do well with this oven. With that said, let me add that you will need to verify that your existing profiles will work as well with the BGAs you are processing. This will require instrumenting boards with thermocouples and measuring their temperature responses. If the components/boards you are using are just too expensive for this, I would suggest getting some dummy parts and board and use them. Just be sure that the dummy components/boards accurately represents the board you are using in production.
Hope this helps,
John Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Crain, Peter (GE Energy)
Sent: Monday, September 20, 2004 4:07 PM
To: [log in to unmask]
Subject: [TN] New reflow oven needed for BGAs???
Hi all,
We are looking at placing BGAs. We currently use a 5 zone reflow oven that
does a great job of soldering all other components. In fact, we only have a
few profiles which are used on many products.
Is there a need for more zones when going to BGA? Does size BGA size matter?
Thanks in advance,
Peter
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|