TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steven Creswick <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Date:
Thu, 5 Jun 2014 09:13:39 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
Graham,

Back in the day, we would have approached as much as we could with hybrid
technology.  

Eutectic die attach on ceramic [High temp co-fired ceramic, alumina
substrate within metal package, or Low Temp Co-fired ceramic], etc.  Way
back, there was even eutectic attach for passives - if properly
metallized...

Being in a hermetic package, no conformal coatings...

Being a potentially highly corrosive environment the package is truly put to
the test.  Drawing upon implantable medical technologies [also a corrosive
environment, believe it or not], there are multiple packaging options
available including stainless & titanium.

Just a different persective...

Steve Creswick
Sr Associate - Balanced Enterprise Solutions
http://www.linkedin.com/in/stevencreswick
                         616 834 1883






______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2