TECHNET Archives

May 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Alan Kreplick <[log in to unmask]>
Date:
Tue, 2 May 2000 16:55:48 -0400
Content-type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Alan Kreplick <[log in to unmask]>
Parts/Attachments:
text/plain (49 lines)
Hello Technetters:

I've gone from the WS6536 100% world to IPC's 50% hole fill requirement.
Unfortunately, I have a .150" thick pcb (G10, with many layers of ground) that
must be waved in a selective soldering fixture, that is averaging about 33-50%
hole fill.

The customer is looking at the 50% hole fill spec, and touching up to meet this
requirement (also, they are touching up from the topside and cosmetically
getting 100% hole fill to make them feel happy).

To achieve the current hole fill, my topside temperature leaving the preheaters
is 270F and the bottom-side portions of the board that are exposed to the
preheaters and wave are at 320F (my normal range and that recommended by the OA
flux manufacturer is 180-220F topside).

Also, the speed is 60cm/min (2 f/m), which on my machine equals about a 3 second
dwell @ 482F.

I can get 50% hole fill if I max out my preheaters which gives me a top-side
temp of 320F and bottom-side temp of 370F.  Running a board at these
temperatures just to meet a 50% hole fill requirement doesn't make sense.

My theory: if 50% of a .060" thick board (.030") is OK, then a 25% hole fill of
a .150" thick board (.0375") would also be OK.


Any thoughts???


Al Kreplick
Sr. Mfg. Eng.
Teradyne, Inc.
978-370-1726

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2