Guenter
Your information is not accurate for all VP systems. Note that the term
Condensation Soldering (CS) also applies.
Our system, for SAC alloy melting at 218 DegC uses a 230 DegC boiling point
fluid. The actual temperature delta over melting / eutectic is less than 5
DegC.
In conventional convection ovens, the temp delta may well be 30 to 50DegC
over melting/eutectic, and this might explain the 270 DegC comment. There
are fluids with a 270 DegC boiling point, but they should not be required in
this process.
With a VP or CS type system, the vapour simply condenses onto all surfaces
that are colder than it, thus it is fast but controllable.
Regards Graham Naisbitt
[log in to unmask] <mailto:[log in to unmask]>
Concoat Limited
Alasan House, Albany Park
Camberley GU16 7PH - UK
www.concoat.co.uk <http://www.concoat.co.uk>
Phone: +44 1276 691100
Fax: +44 1276 691227
Mobile: +44 79 6858 2121
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Guenter Grossmann
> Sent: 14 February 2002 16:44
> To: [log in to unmask]
> Subject: [TN] Antw: [TN] Vapor Phase Soldering ReVisited!
>
>
> Jim
>
> I believe the VP is still a good principle. However, the
> industrial partner in LEADFREE that runs the VP trials told me
> that he has to use a liquid with a boiling point of 270 deg.C and
> that there is nothing available that boils around 230 deg.
> I had problem to believe this but also after asking again I got
> the same answer.
>
> Best regards
>
> Guenter
>
> .
>
> EMPA
> Swiss Federal Institute for Materials Testing and Research
> Centre for Reliability
> Dipl. Eng. Guenter Grossmann
>
> 8600 Duebendorf
> Switzerland
>
> Phone: xx41 1 823 4279
> Fax : xx41 1823 4054
> mail: [log in to unmask]
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|