Kevin,
     Our FEA study concluded that the most likely source of thermal stress
resulting in a crack was the cooldown / reheating between the waves of a dual
wave solder system.  If the temperature shock upon entering the first wave is
less than 100C and the temperature drop between waves was kept to less than
62C, then the data predicted no cracking would occur.  We were able to
consistently create cracked capacitors by performing solder joint touch up
with a solder iron.  Only hot-air touch up would allow the right ramp rates
for crack-free caps.

Jon Moore

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2