TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
Jim Marsico 516-595-5879 <[log in to unmask]>
Date:
Wed, 13 Aug 1997 12:54:00 -0400
MIME-version:
1.0
Content-type:
TEXT/PLAIN; CHARSET=US-ASCII
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Jim Marsico 516-595-5879 <[log in to unmask]>
Parts/Attachments:
TEXT/PLAIN (30 lines)
Technetters:

I won't bother you with the gory details, but I'm looking a source for the
following materials:

        Solder coated copper balls approximately 0.8 mm in diameter

        Pb46-Sn46-Bi8 solder balls 0.8mm in diameter

        Water soluble solder paste with an alloy of Pb46-Sn46-Bi8.

Any suggestions?

Thanks,

Jim Marsico
(516) 595-5879
[log in to unmask]

                        ********************************
                        *       ______   _   _  _____  *
                        *      / ___  | | | | | _____  *
                        *     / /___| | | | | | _____  *
                        *  __/  ____  | | | | |______  *
                        * |____/    |_| |_| |________| *
                        *                              *
                        *         SYSTEMS, INC.        *
                        ********************************


ATOM RSS1 RSS2