Hi,
No, I'm not. (sorry)
Argon isn't going to etch epoxy or metal, and with only 100 watts is barely going to clean
organics. Silicon is always tough. I like Rudy's suggestion (I usually do) but if your going
to plasma use O2 with a dash (2%) of CF4 and crank up that power to like, say, 1000 watts.
Chuck Brummer
Acuson
Good Luck!
[log in to unmask] wrote:
> Why do all that plasma cleaning of assemblies, dosen't plasma etch metal and
> desmear epoxies, sounds like a lot of compoinents could be affected over time.
> Could you just wash the bds. in a water spray sopinafer type machine?
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|