TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Roberts, Jon" <[log in to unmask]>
Date:
Wed, 21 Feb 2007 10:54:12 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ted Tontis <[log in to unmask]>
Subject:
From:
Ted Tontis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (98 lines)
Jim,
	Here is what I use, you start out at 40 degrees C in an oven that is at less then 5% relative humidity for 192 hours. Depending on how large the part is and how much moisture it has absorbed, it could go longer then that. Do not go above 45 degrees C or the tape will go bad. It is important to note that the peel back force on your reeled components will increase. if this isn't a problem then bump the temp up a little to 125 degrees C. 
	This information was posted on tech net some time ago and I printed it out and taped it to our oven. I tried finding the original post in the archive section of TN but couldn't find it so I gave the short version. 


Ted

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roberts, Jon
Sent: Wednesday, February 21, 2007 10:13 AM
To: [log in to unmask]
Subject: Re: [TN] Baking Moisture sensitive devices that are on a real.

Jim, 
Our experience says no to baking on tape and reel or tubes (tape and reel
not marked with any temperature information will start to melt).  I had to
find waffle trays from our stack of them with the space and height to
accommodate the parts (will not be exact). We removed the parts from the
tape and reel near the temperature chamber, place them inside two trays (one
on top of the other),taped together using kapton tape and then place into
the temperature chamber.  
We have at least two oops leaving on tape and reel or in tubes so hopes this
helps, Jon


-----Original Message-----
From: West, Jim [mailto:[log in to unmask]] 
Sent: Wednesday, February 21, 2007 9:02 AM
To: [log in to unmask]
Subject: [TN] Baking Moisture sensitive devices that are on a real.

We have a PQFP-64 that we received on a real and the moisture sensitivity
level is 3.  The package has been opened and has exceeded the maximum
exposure time and requires the component to be baked for a minimum of 8hrs @
125°C.  In the past we received these on trays and baking them was not an
issue.  Can I bake these while on the reel?  Do we need to extend the baking
time?
 
Thanks,
 


Jim West
Engineering Manager
Nexergy Inc.
www.nexergy.com
tel: (614) 351-6216
fax: (614) 324-1979



This email message and all attachments transmitted with it are intended
solely for the use of the addressee(s) and may contain legally privileged,
protected or confidential information. If you believe that you have received
this message in error, please notify the sender immediately by email reply
and please delete this message from your computer and destroy any copies.

--------------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------------------------
Confidentiality Notice

This e-mail and any attachment(s) are intended for the individual or entity to which this email is addressed and may contain information that is confidential.  If you are not the intended recipient or an employee or agent responsible for delivering this e-mail to the intended recipient, please be aware that any dissemination, distribution or copying of this communication is strictly prohibited.  If you have received this in error, please notify the sender by telephone at 604.430.4336 or by return e-mail, and please delete or destroy all copies of this communication.  Thank you!

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2