We have found some internal fab defect (cracking at one of the inner layer)
which we don't know is due to assembly process or fab process induced.

If I were to create a Thermal shock profile to precipitate defect on a
loaded board How can I come out with? I have decided to use -10C to +70C, 10
minutes soaks, +/-20C/minute ramps, 12 cycles which will give a test
duration approx. 3.6 hours.

Any comments will be highly appreciated. All the failed one were found
during ICT testing hence decided to send all lot.

re,
Ken Patel

______________________________________________________
Ken Patel                       Phone:  (408) 490-6804
1708 McCarthy Blvd.             Fax:    (408) 490-6859
Milpitas, CA 95035

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2