Sender: |
|
X-To: |
|
Date: |
Thu, 30 Aug 2012 13:34:03 +0200 |
Reply-To: |
|
Message-ID: |
<07040D8E269C468A8F842E49752901D0@sala60be2e1546> |
Subject: |
|
From: |
|
Content-Transfer-Encoding: |
quoted-printable |
In-Reply-To: |
|
Content-Type: |
text/plain; charset="iso-8859-1" |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
Hi Graham,
very helpfull Data Book, well done !!!
Thank you
Gabriele
-----Messaggio originale-----
Da: TechNet [mailto:[log in to unmask]] Per conto di Graham Naisbitt
Inviato: giovedì 30 agosto 2012 11.21
A: [log in to unmask]
Oggetto: Re: [TN] Cloudy Conformal Coating
Hi Blair
This might be a little late but, as I used to be involved in the manufacture
of this product, the quick and easy fix is to up the amount of thinners -
BUT, you might need another coat to retain the desired thickness.
The condition I know of as Milking or Blooming - it is trapped humidity.
This is why "wet-back" spray booths are a really bad idea - great for
solvent filtration, but troublesome for the finish.
You really should control your humidity to around 60%RH - too low causes ESD
issues. A de-humidifier won't cost much and makes life easier. Moisture
traps in the air line are essential.
You might like to download a copy of our Facts & Data Book on Conformal
Coating from:
http://www.gen3systems.com/techshot-Conformal_Coating.php
I hope this helps
Graham Naisbitt
Gen3 Systems
On 29 Aug 2012, at 15:03, Blair Hogg wrote:
> I'm hoping that Technetters can share some light on an issue that we
occasionally experience here - we coat some of our boards with 1B73
conformal coating, for some we have a spary machine, others a sprayed by
hand.
>
> Every so often we will process some board through coating and they will
have a cloudy / milky appearance in the coating. We have been told
previously that this happens when humidity is up, since our manual spray
coating area is not in an air-conditioned environment.
>
> Anyone else ever have this problem? How did you fix it?
>
> Thanks,
>
> Blair
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|