Hi,

 Would this be an indication of:

1. Problem in PCB fab process.

2. Problem with elevated temps or rework induced issue.

 Both???

If we assume it is high P at the interface is it from the fab house process
or the result of a diffusion / solution of soldering materials.

 Enquiring Minds want to Know!

Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Wednesday, October 27, 2010 11:01 AM
To: [log in to unmask]
Subject: Re: [TN] Cracks in BGA solderjoints

Dovarish Vladimirowitch,
 Black pad failure is a brittle separation.
Werner

 


 

 

-----Original Message-----
From: vladimir Igoshev <[log in to unmask]>
To: TechNet E-Mail Forum <[log in to unmask]>; Werner Engelmaier
<[log in to unmask]>
Sent: Wed, Oct 27, 2010 10:41 am
Subject: Re: [TN] Cracks in BGA solderjoints


Werner, 



Sorry but I could keep quiet. It;s not a Black pad, but Brittle fracture

Vladimir



SENTEC Testing Laboratory Inc.

11 Canadian Road, Unit 7.

Scarborough, ON M1R 5G1

Tel: (416) 899-1882

Fax: (905) 882-8812

www.sentec.ca



-----Original Message-----

From: Werner Engelmaier <[log in to unmask]>

Sender: TechNet <[log in to unmask]>

Date:         Wed, 27 Oct 2010 10:21:07 

To: <[log in to unmask]>

Reply-To: TechNet E-Mail Forum <[log in to unmask]>,

        Werner Engelmaier <[log in to unmask]>

Subject: Re: [TN] Cracks in BGA solderjoints



 Hallo Günter,

Wie geht's?

The separation is classical 'ENIG 'Black Pad'—separation between Ni and IMC 

layers with dark area being high P concentration; the micro-voids are not
[these 

voids do not look like Kirkendall voids].



 I do not know what you mean be "cracks are somewhere in the width of the
solder 

joint"--I do  not see any cracks in the solder, just those voids.

Werner





 



 



-----Original Message-----

From: Grossmann, Guenter <[log in to unmask]>

To: [log in to unmask]

Sent: Wed, Oct 27, 2010 3:36 am

Subject: [TN] Cracks in BGA solderjoints





Hi Technetters







I have an effect in BGA solder joints that I have never seen before.



In microsections and in FIB preparations I see cracks between the IMC and a 



slightly darker region towards the Ni which I assume to be a P enriched zone
of 



the Ni. However, the cracks are somewhere in the width of the solder joint
and 



they are quite short running out to a row of pores that look somehow like 



Kirkendall voids.



Is there still a possibility to place one or two pictures? Kim's IPC site 



doesn't work.







Best regards







Günter 















______________________________________________________________________



This email has been scanned by the MessageLabs Email Security System.



For more information please contact helpdesk at x2960 or [log in to unmask] 



______________________________________________________________________







---------------------------------------------------



Technet Mail List provided as a service by IPC using LISTSERV 15.0



To unsubscribe, send a message to [log in to unmask] with following text in



the BODY (NOT the subject field): SIGNOFF Technet



To temporarily halt or (re-start) delivery of Technet send e-mail to 



[log in to unmask]: SET Technet NOMAIL or (MAIL)



To receive ONE mailing per day of all the posts: send e-mail to 



[log in to unmask]: SET Technet Digest



Search the archives of previous posts at: http://listserv.ipc.org/archives



Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for 



additional information, or contact Keach Sasamori at [log in to unmask] or 



847-615-7100 ext.2815



-----------------------------------------------------





 



______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask] 

______________________________________________________________________



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for 

additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------




 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2