Tom -
I don't recommend using polyimide as a standard for the following
reasons:
1. Cost -- the last time I checked polyimide was 20-50% more than FR-4
2. Fabricators -- not all fabrication houses can produce polyimide
boards requiring you to qualify more suppliers.
3. Assembly issues - polyimide seems to require more process control
than FR-4 to achieve the same results ( pre-bake, etc.)
If you need dimensional stability over a wide temperature range, I suggest
you look at G-tek or other tetra-functional FR-4 materials they may be a
better choice.
Jeffrey McGlaughlin
Designer
Battelle Memorial Inst.
Columbus Ohio
-----Original Message-----
From: Tom Lambert [SMTP:[log in to unmask]]
Sent: Friday, March 13, 1998 4:58 PM
To: [log in to unmask]
Subject: [TN] FR4 vs Polyimide
>
>Am trying to decide which to standardize on - would appreciate
info, pros
>and cons, for each.
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|