Hi Technet,
We are having a problem concern to trip coating. Details such as:
Material: Humiseal 2A64 Part A
Humiseal 2A64 Part B
Thinner 64
Dynaloy Dynasolve 190 (GEL 190)
Mixer 200 gram Humiseal 2A64 Part A and 200 gram Humiseal 2A64 Part B, stir them , after pour 75 gram Thinner 64 to this mixer.
Viscosity: 20 seconds.
Method: Using Dynaloy Dynasolve 190 to strip coating on PWA (Immerse PWA into Dynaloy Dynasolve 190 about 2 hours)
We can not strip the coating layer by this method.
Would you please help us to solve this problem.
Thanks and best regards,
***************************
Nguyen Hoang Luan
QC&Training Supervisor
Spartronics VietNam Co, Ltd.
No.3, Street No.6, VSIP
Th An Dist., BDuong Prov., VN
Tel: (84-650) 784 890
Fax: (84-650) 784 891
Mobile: 090.3.667448
Email: [log in to unmask]
***************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|