TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Neil Atkinson <[log in to unmask]>
Date:
Wed, 3 Oct 2001 17:57:01 +0100
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (71 lines)
I have read all the stuff on black pad etc. and my advice would be to try
immersion tin.  Immersion tin is an easier process for the board shop to
control and therefore you have lower odds of receiving a board with plating
problems.  I would only use ENIG if you NEED it e.g. edge connectors etc.

Immersion silver I have seen go black and unsolderable, that was some time
ago though and things may have improved?!?!?  I have never had a
solderability issue with an immersion tin PCB.

If I were you I would try immersion tin - in my experience it has as good a
shelf life as ENIG if stored reasonably and is much more reliable from an
assemblers point of view, because as you are finding it wastes a hell of a
lot of time when you get solderability problems just finding out who to
blame!!!

One other thing, I am no expert on ENIG (other than the heartaches it
causes) but I have had boards in the past with solderability problems due to
voids in the nickel plating allowing the copper and gold to diffuse
resulting in unsolderable finish - could you be seeing this??

Neil

-----Original Message-----
From: Kirsch, Clif [mailto:[log in to unmask]]
Sent: 02 October 2001 21:45
Subject: ENIG v Immersion Ag


We are running into solderability issues with ENIG boards, especially under
dense (500+ pins) BGA devices. Once the BGA is removed some of the pads
indicate they did not / will not wet.

Does anyone have experience with immersion silver finished boards from a
reliability and NEBS compliant standpoint? Also are there surface resistance
issues for test pads that are not reflowed with solder?

Clif Kirsch
Mfg Eng

#####################################################################################
Attention:

This message is for the named person's use only.  It may contain confidential,
proprietary or legally privileged information.  No confidentiality or privilege
is waived or lost by any mistransmission.  If you receive this message in error,
please immediately delete it and all copies of it from your system, destroy any
hard copies of it securely and notify the sender.  You must not, directly or
indirectly, use, disclose, distribute, print, or copy any part of this message
if you are not the intended recipient. STADIUM GROUP PLC and any of its subsidiaries
each reserve the right to monitor all e-mail communications through its networks.
Any views expressed in this message are those of the individual sender, except where
the message states otherwise and the sender is authorised to state them to be the
views of Stadium Group Plc. or one of its subsidiaries.

Although this message has been scanned by MailMarshall for known viruses and
inappropriate content, we recommend that recipients employ appropriate measures on
their systems to intercept any such material.

Thank You - Stadium Group Plc., IT Department - Tel: +44 (0)1429 266544
#####################################################################################

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2