TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Kasprzak, Bill (sys) USX" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 26 Mar 2001 07:46:54 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (57 lines)
Anybody look on a container of decaf coffee lately? One of the ingredients
used in the process, is Methlylene Chloride. See web info below

As with all decaffeination processes, the direct method begins with soaking
green unroasted beans. The beans are then flushed with methylene chloride
(DCM), a solvent that is generally used in direct contact with the beans. As
the DCM soaks through all parts of the bean, the caffeine is drawn out. The
U.S. Food and Drug Administration (FDA) considers the DCM residual levels in
this decaffeination process low enough to be acceptable. The FDA, however,
and the National Cancer Institute have both linked DCM to cancer in
laboratory animals. In 1989 the FDA banned DCM for use in cosmetics and hair
sprays.

Who says, not easy to get.

No decaf for me.

Bill Kasprzak
Moog Inc.

> -----Original Message-----
> From: Larry J. Fisher [SMTP:[log in to unmask]]
> Sent: Sunday, March 25, 2001 10:09 PM
> To:   [log in to unmask]
> Subject:      Re: [TN] Epoxy Ink Stripper...
>
> The best stripping solvent I know of for cured epoxy materials is
> methlylne
> chloride. The best methlyene chloride "strippers" are the old paint
> strippers
> that contain methylene chloride and wax (when the methylene chloride
> starts
> to evaporate, the wax forms a barrier at the surface to prevent further
> evaporation - therefore the methylene chloride can strip further).
>
> Methlyene chloride is on the "bad news" list these days and is not easy to
>
> get. I'm not sure if you can even get the methylene chloride based paint
> strippers any more. Furthermore, the methylene chloride can also do a
> "number" on the butter coat of your laminate. Good Luck!
>
> Regards,
>
> Larry Fisher
>
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2