Carl,

"It depends"!!!!!!

1. High current crimped connections would become more reliable (particularly in harsh conditions).
    Failures can be very catastrophic.

2. Fold over/upset crimps can become more reliable with solder (particularly in harsh conditions).

3. Soldering 3 or 4 sided compression crimps would cause more problems than they would solve.

These are general rules of thumb so be careful and evaluate the situation carefully

This is from 35+ plus years of dealing with field failures.

David A. Douthit
Manager
LoCan LLC

Carl VanWormer wrote:

> We have a customer who insists that we solder our crimp connectors (after
> crimping).  He has had corrosion problems and is convinced that this is the
> best solution.  Is this a good thing?  Are there any downsides we should
> point out to help educate him?
>
> Carl Van Wormer
> Cipher Systems
> 1815 NW 169th Place, Suite 5010
> Beaverton, OR  97006
> Phone (503)-617-7447    Fax (503)-617-6550
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2