TECHNET Archives

November 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Anil Kher <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 23 Nov 1999 09:43:35 +0530
Content-Type:
multipart/alternative
Parts/Attachments:
text/plain (475 bytes) , text/html (1225 bytes)
mipl1Dear All,

While measuring Gold plating thickness on FR-4 material - Bromine correction is used - this ends up with lower than actual thickness in our case - Why is this done and is Bromine a neccessary component of all FR-4 laminates?
Please reply earliest as my Gold plate thickness of 0.5 mic is measuring same on Fundamental Parameters but as low as 0.3 microns with Bromine correction and my customer is pissing mad

Anil Kher