TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"James R. Paulus" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 16 Nov 1998 14:37:31 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (39 lines)
ed:
the following is an explanation of the referenced slash sheets to 4101:

L/24:  note the Tg range of 150 to 200°, which translates to FR4's known as
high temperature or high performance, such as PCL's 370 or AlliedSignal's 406
or Nelco's 4105-6.  Their chemical makeup is generally 100% multifunctional
resin (un-blended with difunctional.)

(fyi, Polyclad's "standard material 1226FR is covered by /21.)

L/25:  this covers GE's GETEK version of a high temperature FR4, which has a
resin copolymer containing the thermoplastic PPO for lower Dielectric
Constant.

L/26:  Not a tetrafunctional.  This covers the BT type materials when you want
to use them for a drawing calling out type GF.  Note that BT is a blend of a
Cyanate Ester type resin with epoxy, which is the point of the "modified ...
epoxy resin" reference.  This slash sheet also allows other epoxy-based
materials with a higher Tg (170-220°) besides BT to be used.

FYI, slash 30 is intended to apply to BT materials also.  The ID Reference of
"MIL-S-13949/26 - GFT" is an error.  It should refer to 13949/24 and 26 - Type
GMN.

Hope this clears up some questions.
jimpaulus

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2